登录    注册    忘记密码

期刊文章详细信息

裂纹损伤混凝土力学性质试验与PFC模拟研究    

Experimental study on mechanical properties of concrete with crack damage and PFC simulation

  

文献类型:期刊文章

作  者:戎虎仁[1] 王海龙[1] 曹海云[2] 赵岩[1] 张旭恒[3] 穆柏林[1] 王占盛[4] 冯梅梅[5] 王子河[6]

RONG Huren1a, WANG Hailong1a, CA O Haiyun1b, ZHAO Yan1a, ZHANG Xuheng2, MU Bailin1a, WANG Zhansheng3, FENG Meimei4, WANG Zihe5(1a.School of Civil Engineering; b.School of Architecture and Art, Hebei University of Architecture, Zhangjiakou 075000, China; 2.Institute of Civil Engineering, Beijing Jiaotong University, Beijing 100044, China; 3.Tie Er Yuan in Institute of Science and Technology, Chengdu 610000, China; 4.State Key Laboratory for Geomechanics and Deep Underground Engineering, China University of Mining and Technology,Xuzhou 221008,China; 5.Institute of Water Resources for Pastoral Area, Hohhot 021002, China)

机构地区:[1]河北建筑工程学院土木工程学院,河北张家口075000 [2]河北建筑工程学院建筑与艺术学院,河北张家口075000 [3]北京交通大学土木建筑工程学院,北京100044 [4]中铁二院科学技术研究院,四川成都610000 [5]中国矿业大学深部岩土力学与地下工程国家重点实验室,江苏徐州221008 [6]水利部牧区水利科学研究所,内蒙古呼和浩特021002

出  处:《混凝土》

基  金:国家自然基金青年基金(51404266);河北省教育厅科技青年基金(QN2016066);张家口市科学技术和地震局指令项目(1611061A);河北建筑工程学院校级基金(B-201602);中国中铁重点科研课题(2016-重点-27)

年  份:2018

期  号:3

起止页码:8-12

语  种:中文

收录情况:BDHX、BDHX2017、CAS、CSA、CSA-PROQEUST、JST、RCCSE、ZGKJHX、核心刊

摘  要:通过室内试验对恒定倾角(45°)裂纹损伤试件裂纹长度差异对混凝土力学性研究,并结合PFC颗粒流数值模拟软件分析结果裂纹扩展规律,进一步阐述其破坏形态及机理。研究表明:(1)裂纹损伤试件强度随着裂纹长度增大逐渐降低,降低速率先减小后增大;弹性模量随着裂纹长度增大逐渐降低,其中降低速率先增大后减小最后再降低。(2)裂纹长度为10 mm时,试件破坏形态为整体破坏;裂纹长度为20~30 mm时,试件破坏沿着初始裂纹扩展方向破坏,部分沿着初始裂纹反方向破坏,表现出裂纹部分影响破坏形态;裂纹长度≥40 mm,试件完全沿着初始裂纹扩展方向破坏,无反向裂纹产生。

关 键 词:损伤混凝土  力学性质 裂纹长度  PFC模拟  

分 类 号:TU528.01]

参考文献:

正在载入数据...

二级参考文献:

正在载入数据...

耦合文献:

正在载入数据...

引证文献:

正在载入数据...

二级引证文献:

正在载入数据...

同被引文献:

正在载入数据...

版权所有©重庆科技学院 重庆维普资讯有限公司 渝B2-20050021-7
 渝公网安备 50019002500408号 违法和不良信息举报中心