登录    注册    忘记密码

期刊文章详细信息

Effects of mechanical activation and oxidation-reduction on hydrochloric acid leaching of Panxi ilmenite concentration  ( EI收录 SCI收录)  

机械活化和氧化-还原处理对攀西钛铁矿精矿盐酸浸出的影响(英文)

  

文献类型:期刊文章

作  者:谭平[1] 胡慧萍[2] 张黎[2]

机构地区:[1]湖南机电职业技术学院生物化工系,长沙410151 [2]中南大学化学化工学院,长沙410083

出  处:《Transactions of Nonferrous Metals Society of China》

基  金:Project(2009FJ3082)supported by Research Project of Science and Technology in Hunan Province,China;Project(2007CB613606)supported by the National Basic Research Program of China

年  份:2011

卷  号:21

期  号:6

起止页码:1414-1421

语  种:中文

收录情况:AJ、CAS、CSA、CSA-PROQEUST、CSCD、CSCD2011_2012、EBSCO、EI、IC、INSPEC、JST、SCI(收录号:WOS:000293005400034)、SCI-EXPANDED(收录号:WOS:000293005400034)、SCIE、SCOPUS、WOS、ZGKJHX、普通刊

摘  要:The effects of oxidation-reduction treatment and mechanical activation on the hydrochloric acid leaching performance of Panxi ilmenite concentration were investigated.The results show that both of oxidation-reduction treatment and mechanical activation significantly accelerate the extraction of Fe,Ca and Mg from Panxi ilmenite concentration;however,the CaO and MgO contents of the calcined residues obtained from oxidized-reduced ilmenite concentration are higher than the standard values required by chlorination process.The Ca and Mg in oxidized-reduced ilmenite concentration can be leached much faster after mechanical activation,yielding a synthetic rutile which meets the requirements of chlorination process containing 90.50% TiO2 and 1.37% total iron as well as combined CaO and MgO of 1.00%.The optimum oxidation and reduction conditions are as follows:oxidization at 900 ℃ in the presence of oxygen for 15 min and reduction at 750 ℃ by hydrogen for 30 min.

关 键 词:ilmenite concentration  mechanical activation  OXIDATION REDUCTION hydrochloric acid leaching  

分 类 号:TD951]

参考文献:

正在载入数据...

二级参考文献:

正在载入数据...

耦合文献:

正在载入数据...

引证文献:

正在载入数据...

二级引证文献:

正在载入数据...

同被引文献:

正在载入数据...

版权所有©重庆科技学院 重庆维普资讯有限公司 渝B2-20050021-7
 渝公网安备 50019002500408号 违法和不良信息举报中心